Fiber Laser Cutting Thickness Chart: 1 kW to 30 kW

Quick answer: a 1 kW fiber laser cuts 3 mm stainless, 6 mm carbon steel and 2 mm aluminium. At 6 kW those numbers become 15 / 22 / 12 mm. Above 12 kW the maximum thickness barely moves — what changes is the quality-limit thickness, the point where cut speed is still economical for production. Most buyers over-specify watts and under-specify gas supply and chiller capacity.

1. Maximum thickness by power

PowerStainless (N₂)Carbon steel (O₂)Aluminium (N₂)Brass / copper
1 kW3 mm6 mm2 mm1 mm
2 kW5 mm10 mm4 mm2 mm
3 kW8 mm14 mm6 mm3 mm
6 kW15 mm22 mm12 mm6 mm
12 kW25 mm30 mm20 mm10 mm
20 kW40 mm40 mm30 mm16 mm
30 kW60 mm50 mm40 mm22 mm

These are single-pass maximums with a clean edge. Going 20% thicker than the table is possible on carbon steel with oxygen, at the cost of a rough lower edge that needs a second operation.

2. Maximum thickness is not the useful number

Cut speed falls faster than thickness rises. On 6 kW stainless, 6 mm cuts at 3.5 m/min while 15 mm cuts at 0.4 m/min — the same machine, one ninth the speed. The quality-limit thickness is where throughput stops paying for the power bill: roughly half the maximum thickness for stainless, and two thirds for carbon steel.

PowerQuality-limit thickness (stainless)Speed at that thickness
3 kW4 mm6.0 m/min
6 kW8 mm3.0 m/min
12 kW14 mm1.8 m/min
20 kW22 mm1.2 m/min

3. What else limits thickness

  • Nitrogen supply. 15 mm stainless needs 18–22 bar at the nozzle. A 30 bar liquid tank and a 3-stage regulator are part of the machine purchase, not an accessory.

  • Chiller capacity. Every additional 3 kW of source adds roughly 8 kW of heat to reject. Undersized chillers derate the source in summer, and the symptom looks like “the machine got weak”.

  • Nozzle diameter. Thick-section cutting needs 2.0–3.0 mm single nozzles. A 1.2 mm nozzle that works perfectly at 3 mm will starve at 12 mm regardless of power.

  • Beam parameter product. High-power sources with poor BPP produce a fat spot that cannot form a narrow keyhole, so the extra watts go into widening the kerf instead of deepening it.

4. Choosing power for a real production mix

Take the 90th percentile of your thickness mix, not the maximum, and size to the quality-limit thickness. A shop that cuts 80% 2 mm and 20% 8 mm stainless does not need 12 kW. A 6 kW machine handles the 8 mm at 3.0 m/min and the 2 mm at 25 m/min, and saves both capital and nitrogen.

The exception is thick-plate work where one 25 mm part defines the contract. Then buy for the 25 mm and accept that the machine is oversized for everything else — but budget the nitrogen, because a 20 kW source on 25 mm stainless consumes gas at a rate that surprises first-time buyers.

Frequently asked questions

Can a 3 kW laser cut 10 mm stainless?

It can cut it, at roughly 0.35 m/min, but the edge quality degrades and dross becomes likely. The honest answer is that 3 kW is a 6–8 mm stainless machine.

Why does carbon steel cut thicker than stainless at the same power?

Because oxygen does the work. In carbon steel the exothermic reaction adds energy to the cut; stainless is cut with inert nitrogen, so the laser supplies 100% of the energy and the molten metal is only blown out.

Does more power always mean faster cutting on thin sheet?

No. Below about 2 mm, acceleration and the machine’s dynamics dominate. A 12 kW machine and a 3 kW machine cut 1 mm stainless at nearly the same speed because neither ever reaches full power on the part.

Related reading

Intouchray has manufactured industrial fibre laser cutting, welding, cleaning and cladding machines in Dongguan, Guangdong, China since 2001, with additional bases in Wuhan and Korea. Minimum order is one machine, built to order.

About the Author