title: "Laser Cutting Dross: Diagnosis Table for Oxygen and Nitrogen"
url: https://www.intouchray.com/laser-cutting-dross-oxygen-nitrogen-parameters/
date: 2026-11-10
modified: 2026-11-10
lang: en
author: "Sales11@taiyilaser.com"
description: "Quick answer: dross type tells you which parameter is wrong. Hard, welded-on dross on the bottom edge means the gas could not push the melt out. Soft, wipes-off dross means..."
categories:
  - "Technical Support"
word_count: 426
---

# Laser Cutting Dross: Diagnosis Table for Oxygen and Nitrogen

[Home](https://www.intouchray.com) - [Technical Support](https://www.intouchray.com/category/technical-support/) - Laser Cutting Dross: Diagnosis Table for Oxygen and Nitrogen

**Quick answer:** dross type tells you which parameter is wrong. Hard, welded-on dross on the bottom edge means the gas could not push the melt out. Soft, wipes-off dross means the cut was too fast for the gas to finish. Upper-edge dross means the focus is too high. Changing power is almost never the right first move.

## 1. Diagnosis table

| Dross type | Gas | Cause | Change first |
| ---------- | --- | ----- | ------------ |
| Hard, welded, bottom | Nitrogen | Pressure too low | +2 bar |
| Hard, welded, bottom | Oxygen | Speed too high | −10% speed |
| Soft, wipes off | Either | Speed too high | −8% speed |
| Fine beads, whole length | Nitrogen | Focus too high | Focus −1 mm |
| Dross on one side only | Either | Nozzle off-centre | Re-centre to 0.1 mm |
| Dross at corners only | Either | Acceleration drop | Corner dwell or CAM rounding |
| Upper-edge rewelded slag | Oxygen | Pressure too high | −0.3 bar |

## 2. The steps that actually work

- **Check the nozzle first.** A nozzle 0.1 mm off-centre produces dross on one side of the kerf only, and it mimics a focus problem.

- **Then check focus.** A 0.5 mm focus error changes the kerf and the dross pattern more than a 2 bar gas change.

- **Then gas.** Nitrogen dross is a pressure problem; oxygen dross is a pressure-versus-speed balance problem.

- **Power last.** If gas, focus and nozzle are right and dross persists, the material may need a different recipe — not more watts.

## 3. Material-specific notes

Aluminium drosses more than steel because its oxide melts at 2072 °C — far above the metal — so oxide islands survive in the kerf and act as anchors for dross. Higher pressure and a slightly negative focus help.

Hot-rolled carbon steel with mill scale behaves like a different material from pickled steel. Expect to lower speed 15% on scale, and expect dross that looks like a speed problem when the real cause is scale absorbing energy at the surface.

## Frequently asked questions

### Why does dross appear only on the last 20 mm of a cut?

Gas supply pressure drop. A regulator sized for average flow cannot hold 18 bar at the end of a long cut on a small accumulator. Check the gauge during the cut, not before it.

### Can dross be removed instead of prevented?

Mechanically yes, but it doubles handling cost. If more than 5% of parts need de-drossing, the process is losing money against a one-hour parameter trial.

### Does higher power always reduce dross?

No. On nitrogen cutting, extra power widens the kerf and makes it easier for the gas to clear — but on thin sheet it also increases the chance of the melt rolling under. Fix gas and focus first.

## Related reading

- [Kerf width and 0.1 mm tolerance](https://www.intouchray.com/laser-cutting-kerf-width-tolerance-parameters/)

- [Assist gas pressure by thickness](https://www.intouchray.com/laser-cutting-assist-gas-pressure-bar-by-thickness/)