3 Cutting Modes to Consider When Buying Laser Cutters for Metals
Industrial laser cutting uses three process modes. Fusion cutting uses nitrogen at 10-25 bar. It produces clean, weld-ready edges. Oxidation cutting uses oxygen at 0.3-2.0 bar. The exothermic reaction contributes roughly 60% of cutting energy. This allows faster speeds on…