Multi-station automatic laser welding in the application of agricultural tools
Multi-station automatic laser welding boosts agricultural tool production by overlapping welding with loading, achieving 450–600 parts per hour versus 160–200 for single-station cells, with 3–4× faster travel speeds, no post-weld grinding, narrow heat-affected zones preserving hardened edges, and payback typically…