The Physics of the Fiber Laser Weld Pool
Fiber laser weld pools are governed by power density (laser power and beam quality, M² ≤ 1.1), material absorptivity at 1,064nm, and workpiece thermal conductivity. Above the keyhole threshold, surface tension, vapour pressure, and Marangoni convection balance to determine penetration,…