title: "Fiber Laser Cutting Thickness Chart: 1 kW to 30 kW"
url: https://www.intouchray.com/fiber-laser-cutting-thickness-power-chart-1kw-30kw/
date: 2026-11-10
modified: 2026-11-10
lang: en
author: "Sales11@taiyilaser.com"
description: "Quick answer: a 1 kW fiber laser cuts 3 mm stainless, 6 mm carbon steel and 2 mm aluminium. At 6 kW those numbers become 15 / 22 / 12..."
categories:
  - "Technical Support"
word_count: 639
---

# Fiber Laser Cutting Thickness Chart: 1 kW to 30 kW

[Home](https://www.intouchray.com) - [Technical Support](https://www.intouchray.com/category/technical-support/) - Fiber Laser Cutting Thickness Chart: 1 kW to 30 kW

**Quick answer:** a 1 kW fiber laser cuts 3 mm stainless, 6 mm carbon steel and 2 mm aluminium. At 6 kW those numbers become 15 / 22 / 12 mm. Above 12 kW the maximum thickness barely moves — what changes is the *quality-limit* thickness, the point where cut speed is still economical for production. Most buyers over-specify watts and under-specify gas supply and chiller capacity.

## 1. Maximum thickness by power

| Power | Stainless (N₂) | Carbon steel (O₂) | Aluminium (N₂) | Brass / copper |
| ----- | ---------------- | ------------------- | ---------------- | -------------- |
| 1 kW | 3 mm | 6 mm | 2 mm | 1 mm |
| 2 kW | 5 mm | 10 mm | 4 mm | 2 mm |
| 3 kW | 8 mm | 14 mm | 6 mm | 3 mm |
| 6 kW | 15 mm | 22 mm | 12 mm | 6 mm |
| 12 kW | 25 mm | 30 mm | 20 mm | 10 mm |
| 20 kW | 40 mm | 40 mm | 30 mm | 16 mm |
| 30 kW | 60 mm | 50 mm | 40 mm | 22 mm |

These are single-pass maximums with a clean edge. Going 20% thicker than the table is possible on carbon steel with oxygen, at the cost of a rough lower edge that needs a second operation.

## 2. Maximum thickness is not the useful number

Cut speed falls faster than thickness rises. On 6 kW stainless, 6 mm cuts at 3.5 m/min while 15 mm cuts at 0.4 m/min — the same machine, one ninth the speed. The quality-limit thickness is where throughput stops paying for the power bill: roughly half the maximum thickness for stainless, and two thirds for carbon steel.

| Power | Quality-limit thickness (stainless) | Speed at that thickness |
| ----- | ----------------------------------- | ----------------------- |
| 3 kW | 4 mm | 6.0 m/min |
| 6 kW | 8 mm | 3.0 m/min |
| 12 kW | 14 mm | 1.8 m/min |
| 20 kW | 22 mm | 1.2 m/min |

## 3. What else limits thickness

- **Nitrogen supply.** 15 mm stainless needs 18–22 bar at the nozzle. A 30 bar liquid tank and a 3-stage regulator are part of the machine purchase, not an accessory.

- **Chiller capacity.** Every additional 3 kW of source adds roughly 8 kW of heat to reject. Undersized chillers derate the source in summer, and the symptom looks like "the machine got weak".

- **Nozzle diameter.** Thick-section cutting needs 2.0–3.0 mm single nozzles. A 1.2 mm nozzle that works perfectly at 3 mm will starve at 12 mm regardless of power.

- **Beam parameter product.** High-power sources with poor BPP produce a fat spot that cannot form a narrow keyhole, so the extra watts go into widening the kerf instead of deepening it.

## 4. Choosing power for a real production mix

Take the 90th percentile of your thickness mix, not the maximum, and size to the quality-limit thickness. A shop that cuts 80% 2 mm and 20% 8 mm stainless does not need 12 kW. A 6 kW machine handles the 8 mm at 3.0 m/min and the 2 mm at 25 m/min, and saves both capital and nitrogen.

The exception is thick-plate work where one 25 mm part defines the contract. Then buy for the 25 mm and accept that the machine is oversized for everything else — but budget the nitrogen, because a 20 kW source on 25 mm stainless consumes gas at a rate that surprises first-time buyers.

## Frequently asked questions

### Can a 3 kW laser cut 10 mm stainless?

It can cut it, at roughly 0.35 m/min, but the edge quality degrades and dross becomes likely. The honest answer is that 3 kW is a 6–8 mm stainless machine.

### Why does carbon steel cut thicker than stainless at the same power?

Because oxygen does the work. In carbon steel the exothermic reaction adds energy to the cut; stainless is cut with inert nitrogen, so the laser supplies 100% of the energy and the molten metal is only blown out.

### Does more power always mean faster cutting on thin sheet?

No. Below about 2 mm, acceleration and the machine's dynamics dominate. A 12 kW machine and a 3 kW machine cut 1 mm stainless at nearly the same speed because neither ever reaches full power on the part.

## Related reading

- [Assist gas pressure by thickness](https://www.intouchray.com/laser-cutting-assist-gas-pressure-bar-by-thickness/)

- [Laser beam quality and the M² factor](https://www.intouchray.com/laser-beam-quality-m2-factor-guide/)